Polymer Property : Charpy Impact Unnotched = 8.10 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 8.10 J/cm²

@Temperature -30.0 °C
38.5 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® HFD4211 PC
Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Charpy Impact Unnotched 8.10 J/cm²

@Temperature -30.0 °C
38.5 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® HFD4211 PC (Asia Pacific)
Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Charpy Impact Unnotched 8.10 J/cm²

@Temperature -30.0 °C
38.5 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® HFD4211 PC (Europe-Africa-Middle East)
Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Charpy Impact Unnotched 8.10 J/cm²
38.5 ft-lb/in²
23; ISO 179/1eU
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, DRY
Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaPr..
Charpy Impact Unnotched 8.10 J/cm²
38.5 ft-lb/in²
ISO 179/1eU
Solvay TECHNYLSTARâ„¢ S 218 V30 PA6, 30% glass filled, DRY
Description: TECHNYLSTARâ„¢ S 218 V30 is based on a patented high flow polyamide 6 resin (TechnylStar), heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is..
Charpy Impact Unnotched 8.10 J/cm²
38.5 ft-lb/in²
DAM; ISO 179/1eU
Solvay Technyl Starâ„¢ S 218 V30 30% Glass Reinforced Nylon 6
Heat stabilized, low viscosity, injection grade.Information provided by Rhodia; Rhodia has been acquired by Solvay.
Charpy Impact Unnotched 8.10 J/cm²
38.5 ft-lb/in²
50%RH; ISO 179/1eU
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66  (Unverified Data**)
25% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G25HS BK117 is a 25% glass fiber reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information p..
Charpy Impact Unnotched 8.10 J/cm²

@Temperature -30.0 °C
38.5 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK261 Nylon 6  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology only from DuPont it provides exceptional welding resistanceInformation ..
Charpy Impact Unnotched 8.10 J/cm²

@Temperature -30.0 °C
38.5 ft-lb/in²

@Temperature -22.0 °F
ISO 179
BASF Ultramid® 7423-2 NF3001 13% Glass Filled PA66 (Conditioned)
Ultramid 7423-2 NF3001 is an impact modified, 13% glass reinforced, heat stabilized injection molding PA6/6.