Mechanical Properties Metric English Comments
Charpy Impact Unnotched 4.00 - 12.0 J/cm²

@Thickness 4.0 mm
19.0 - 57.1 ft-lb/in²

@Thickness 0.16 in
MD; ISO 179-12fn / PA_097
Quadrant Plastic Composites GMT Glass-Mat-Reinforced Thermoplastic
This semi-finished product in panel form was developed primarily as a substitute for metals (steel, aluminum etc.) and its main purchasers can be found in the automotive industry. This is where it i..
Charpy Impact Unnotched 0.800 - 12.0 J/cm²
3.81 - 57.1 ft-lb/in²
Average value: 4.03 J/cm² Grade Count:95
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Charpy Impact Unnotched 7.00 - 12.0 J/cm²

@Temperature -30.0 - -30.0 °C
33.3 - 57.1 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 8.60 J/cm² Grade Count:5
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Charpy Impact Unnotched 12.0 - 12.0 J/cm²

@Temperature -30.0 - -30.0 °C
57.1 - 57.1 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 12.0 J/cm² Grade Count:1
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..
Charpy Impact Unnotched 5.00 - 12.0 J/cm²
23.8 - 57.1 ft-lb/in²
Average value: 8.23 J/cm² Grade Count:15
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
Charpy Impact Unnotched 2.50 - 12.0 J/cm²

@Temperature -40.0 - -20.0 °C
11.9 - 57.1 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 4.81 J/cm² Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..