Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.80 - 5.30 J/cm² | 13.3 - 25.2 ft-lb/in² | Average value: 4.40 J/cm² Grade Count:24 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |
|||
Charpy Impact Unnotched | 2.80 - 5.30 J/cm² @Temperature -30.0 - -20.0 °C |
13.3 - 25.2 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 4.68 J/cm² Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |