Polymer Property : Charpy Impact Unnotched = 17.6 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 3.70 J/cm²
17.6 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 CV-CM 0515 9005/Z Powder-coatable nylon 6.6 for injection molding, 15% ceramic filled
Powder-coatable nylon 6.6 for injection molding, with conductive carbon blackInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 3.70 J/cm²
17.6 ft-lb/in²
ISO 179/1eU
Nilit FRIANYL A63 FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 3.70 J/cm²

@Temperature -40.0 °C
17.6 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL A63 HS-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced
Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 3.70 J/cm²
17.6 ft-lb/in²
DIN 53453
Nilit FRIANYL B63 FK 2010 Nylon 6 for injection molding, 20% glass fiber and 10% glass ball reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 3.70 J/cm²

@Temperature -40.0 °C
17.6 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL C73 TFGV1530 Nylon 6.6/6 for injection molding, 15% PTFE lubricated, 30% glass fiber reinforced
Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 3.70 J/cm²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
Injection Molded; ISO 179
PolyOne Edgetek® ET3500-5002 BK Acrylonitrile Styrene Acrylate + PC (ASA+PC)
The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Charpy Impact Unnotched 3.70 J/cm²

@Temperature -30.0 °C
17.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 50-3019 Polycarbonate, with glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te..
Charpy Impact Unnotched 3.70 J/cm²
17.6 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1-7032-B Polyamide 66, with aramid reinforcement and PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Improved heat resistance.Control disks, cams, sliding elem..
Charpy Impact Unnotched 3.70 J/cm²
17.6 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, DRY
Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This gr..
Charpy Impact Unnotched 3.70 J/cm²
17.6 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Valox® 7062HP PBT
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Charpy Impact Unnotched 3.70 J/cm²
17.6 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific)
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Charpy Impact Unnotched 3.70 J/cm²
17.6 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East)
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Charpy Impact Unnotched 3.70 J/cm²

@Temperature -20.0 °C
17.6 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eU
Borealis Daplen™ MD206U Polypropylene Compound 20% Mineral Filled
Daplen MD206U is a 20% mineral filled polypropylene compound intended for injection molding. MD206U has been developed especially for automotive interior parts that require excellent balance betwee..
Charpy Impact Unnotched 3.70 J/cm²
17.6 ft-lb/in²
ISO 179-1
Unitika BV2120G15 PA66, 15% Glass Fiber Reinforced, Flame Retardant, Dry
Information provided by Unitika Ltd.
Charpy Impact Unnotched 3.70 J/cm²
17.6 ft-lb/in²
IS0179-1:2000
Zhejiang Juner PA66-301-G10 Flame-Retardant & Glass Reinforced, Environmental PA66
Applications: Electric Appliance PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd.
Charpy Impact Unnotched 3.70 J/cm²

@Temperature -30.0 °C
17.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers
Charpy Impact Unnotched 3.70 J/cm²
17.6 ft-lb/in²
ISO 179/IeU
Addiplast Addilene H 210 G20 Polypropylene Homopolymer
Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast.
Charpy Impact Unnotched 3.70 J/cm²
17.6 ft-lb/in²
Conditioned; ISO 179/IeU
Addiplast Addilene J 490 M20F Flame Retardant Polypropylene, 20% Mineral Filled
Flame retardant, mineral filled, with halogensInformation provided by Addiplast.
Charpy Impact Unnotched 3.70 J/cm² - NB
17.6 ft-lb/in² - NB
Average value: 6.18 J/cm² Grade Count:6
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..
Charpy Impact Unnotched 3.70 J/cm²

@Temperature -20.0 °C
17.6 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eU
Borealis Xmod™ K65G3 30% Glass Fiber Reinforced Polypropylene Compound
Xmod K65G3 is a 30% glass fiber reinforced grade intended for injection molding. Xmod K65G3 has been developed especially for the car industry, to be used UTB parts. Xmod K65G3 offers good balance..
Charpy Impact Unnotched 3.70 J/cm²

@Temperature -30.0 °C
17.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss PLASLUBE J-50/10/TF/15/BK Polycarbonate, with glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te..