Mechanical Properties Metric English Comments
Charpy Impact Unnotched 22.0 J/cm² - NB

@Temperature -40.0 - -30.0 °C
105 ft-lb/in² - NB

@Temperature -40.0 - -22.0 °F
Average value: 30.7 J/cm² Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Charpy Impact Unnotched 22.0 J/cm²
105 ft-lb/in²
Ineos ABS Lustran® H801
High heat resistance, PC modified, low emission, increased flow.,Property data per ISO test methods.
Charpy Impact Unnotched 22.0 J/cm²
105 ft-lb/in²
47 HRC
International Mold Steel DHA-World Die Cast & Forging Steel
DHA-World is a high hardenability and high tough general use hot work die steel.Information provided by International Mold Steel
Charpy Impact Unnotched 22.0 J/cm²

@Temperature -30.0 °C
105 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Lanxess Pocan® B 1505 Z 000000 PBT
PBT, non-reinforced, injection molding, extrusion, impact modified
Charpy Impact Unnotched 22.0 J/cm²
105 ft-lb/in²
ISO 179/1eU
Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, Conditioned
Description: TechnylStar Polyamide, 40% mineral filled, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific and North AmericaProduct Appli..
Charpy Impact Unnotched 22.0 J/cm²
105 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s..
Charpy Impact Unnotched 22.0 J/cm²
105 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo..
Charpy Impact Unnotched 22.0 J/cm²
105 ft-lb/in²
ISO 179/1eU
CENTROPLAST CENTRODAL C FG Polyoxymethylene, Food Grade
POM C is a partially crystalline thermoplastic, which is characterized by its excellent machinability, dimensional stability, and chemical resistance.Information provided by CENTROPLAST Engineering ..
Charpy Impact Unnotched 22.0 J/cm²
105 ft-lb/in²
ISO 179
BASF Ultramid® B3M6 30% Mineral Filled PA6 (Dry)
Ultramid B3M6 is a 30% mineral reinforced injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent laser markability.
Charpy Impact Unnotched 22.0 J/cm²
105 ft-lb/in²
ISO 179/1eU
CENTROPLAST CENTROGUARD Polyoxymethylene, Antimicrobial
During the modification with POM CG, antimicrobial substances are included in the basic polyoxymethylene polymer, which provide an effective and long lasting solution against unwanted growth of micr..
Charpy Impact Unnotched 22.0 J/cm² - NB
105 ft-lb/in² - NB
Average value: 28.4 J/cm² Grade Count:133
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..
Charpy Impact Unnotched 22.0 J/cm²
105 ft-lb/in²
ISO 179/1eU
CENTROPLAST CENTRODAL C Polyoxymethylene Copolymer
CENTRODAL C is a versatile material with good chemical resistance, good machinability, and surface slip properties. Applications include sliding components and rollers, toothed wheels, ratchets, an..
Charpy Impact Unnotched 22.0 J/cm²
105 ft-lb/in²
ISO 179/1eU
CENTROPLAST CENTRODAL W Polyoxymethylene
POM W is a semi-crystalline thermoplastic, which is certified in accordance with the regulatory system DVGW, technical regulations, work form W 270 and therefore, is particularly suited for the safe..