Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 100 J/cm² @Temperature -30.0 °C |
476 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Arkema Group Rilsan® Clear G380 Renew Polyamide Rilsan® Clear G830 Rnew is a high performance transparent polyamide partially based on renewable resources. This grade has been specially designed for injection molding applications, ideally suited.. |
|||
Charpy Impact, Notched | 100 J/cm² @Temperature -30.0 °C |
476 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Arkema Group Rilsan® Clear G350 Polyamide Rilsan® Clear G350 is a high performance transparent polyamide. This grade has been specially designed for injection molding applications, ideally suited for optics as high end eyewear frames.Infor.. |