Mechanical Properties Metric English Comments
Charpy Impact, Notched 100 J/cm²

@Temperature -30.0 °C
476 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Arkema Group Rilsan® Clear G380 Renew Polyamide
Rilsan® Clear G830 Rnew is a high performance transparent polyamide partially based on renewable resources. This grade has been specially designed for injection molding applications, ideally suited..
Charpy Impact, Notched 100 J/cm²

@Temperature -30.0 °C
476 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Arkema Group Rilsan® Clear G350 Polyamide
Rilsan® Clear G350 is a high performance transparent polyamide. This grade has been specially designed for injection molding applications, ideally suited for optics as high end eyewear frames.Infor..