Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.540 J/cm² @Temperature 23.0 °C |
2.57 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S CP300 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.540 J/cm² @Temperature -40.0 °C |
2.57 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eA |
Styron INSPIREâ„¢ T710-25 ES PolyPropylene Resin DA Thermoplastic Polyolefin Dow T710-25 ES Polypropylene Resin DAâ„¢ is a high impact TPO with enhanced flow, scratch and mar, and surface aesthetics for excellent molded-in-color appearance for automotive interior applicat.. |
|||
Charpy Impact, Notched | 0.540 J/cm² @Temperature -30.0 °C |
2.57 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Charpy Impact, Notched | 0.540 J/cm² @Temperature 23.0 °C |
2.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Charpy Impact, Notched | 0.540 J/cm² @Temperature 23.0 °C |
2.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
Charpy Impact, Notched | 0.540 J/cm² @Temperature -30.0 °C |
2.57 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
Charpy Impact, Notched | 0.540 J/cm² @Temperature -30.0 °C |
2.57 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Borealis Daplen™ EF103AE Polypropylene TPO Compound Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an.. |