Polymer Property : Charpy Impact, Notched = 12.4 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 2.60 J/cm²

@Temperature 23.0 °C
12.4 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6 GF 65/1M PA6 reinforced with 65% glass fibre
Features: PA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go..
Charpy Impact, Notched 2.60 J/cm²

@Temperature 23.0 °C
12.4 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVAMID® 6 GF 65/2M PA6 reinforced with glass fiber
PA 6 for injection molding, reinforced with 65% of glass fiber, for moldings used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electrotools, hobby to..
Charpy Impact, Notched 2.60 J/cm²

@Temperature 23.0 °C
12.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179
SABIC P6006 Black High Density Polyethylene for Pipes
Product Description: P6006 is a black compound high density (class MRS 8 - PE 80) polyethylene with bimodal distribution of molecular mass. It is specifically designed for Pressure Pipe applicatio..
Charpy Impact, Notched 2.60 J/cm²

@Thickness 102 mm,
Temperature -20.0 °C
12.4 ft-lb/in²

@Thickness 4.00 in,
Temperature -4.00 °F
ISO 179
Premix Thermoplastics PRE-ELEC® PP 1398 Conductive Thermoplastic Compound
PRE-ELEC® PP 1398 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Charpy Impact, Notched 2.60 J/cm²

@Temperature 23.0 °C
12.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179
LG Chemical NT-520 ABS, High Flow, Non Toxic
Information Provided by LG Chem
Charpy Impact, Notched 2.60 J/cm²

@Temperature 23.0 °C
12.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax BTE30-DN00N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact, Notched 2.60 J/cm²

@Temperature 0.000 °C
12.4 ft-lb/in²

@Temperature 32.0 °F
ISO R179
Styron Pulse® A35-110 PC/ABS
PULSEâ„¢ A35-110 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature. The proprietary mass ABS technology of Dow allows these p..
Charpy Impact, Notched 2.60 J/cm²

@Temperature 23.0 °C
12.4 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eA
DSM Akulon® K224-G8 PA6-GF40
40% Glass Reinforced
Charpy Impact, Notched 2.60 J/cm²

@Temperature 23.0 °C
12.4 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eA
DSM Novamid® 1010C2 PA6
Easy Molding Grade
Charpy Impact, Notched 2.60 J/cm²

@Temperature 23.0 °C
12.4 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eA
DSM Novamid® 1017GH33 BK701 PA6-GF33
33% Glass Reinforced, Heat Stabilized, Injection Molding
Charpy Impact, Notched 2.60 J/cm²

@Temperature -30.0 °C
12.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Stanyl® TW363 Nylon 46 (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..