DSM Stanyl® TW363 Nylon 46 (European Grade) (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Unreinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TW363 Nylon 46 (European Grade) (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temperatures Excellent resistance to wear and low friction Outstanding flow for easy processing and exceptional design freedomStanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical propertiesKey Applications: Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensionersE&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliancesInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Water Absorption 11 %
11 %
Sim. to ISO 62
Moisture Absorption at Equilibrium 3.0 %
3.0 %
Humidity Absorption; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.020 cm/cm
0.020 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.020 cm/cm
0.020 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-1/-2
Elongation at Yield 20 %
20 %
ISO 527-1/-2
Tensile Modulus 1.85 GPa
268 ksi
ISO 527-1/-2
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 2.60 J/cm²

@Temperature -30.0 °C
12.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
7.50 J/cm²

@Temperature 23.0 °C
35.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 160 µm/m-°C

@Temperature 20.0 °C
88.9 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 180 µm/m-°C

@Temperature 20.0 °C
100 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Melting Point 295 °C
563 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75-1/-2
Vicat Softening Point 250 °C
482 °F
50°C/h 50N; ISO 306
Glass Transition Temp, Tg 75.0 °C
167 °F
Glass Transition Temperature (10°C/min); ISO 11357-1/-2
Oxygen Index 27 %
27 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Dielectric Constant 3.2

@Frequency 1e+6 Hz
3.2

@Frequency 1e+6 Hz
IEC 60250
3.6

@Frequency 100 Hz
3.6

@Frequency 100 Hz
IEC 60250
Dielectric Strength 25.0 kV/mm
635 kV/in
IEC 60243-1
Dissipation Factor 0.0012

@Frequency 100 Hz
0.0012

@Frequency 100 Hz
IEC 60250
0.0019

@Frequency 1e+6 Hz
0.0019

@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 475 V
475 V
IEC 60112
Descriptive Properties Value Comments
Heat stabilized or stable to heat Yes
High impact or impact modified Yes
Injection molding Yes
Other Extrusion Yes
Platable Yes
Profile extrusion Yes
Without Fillers Yes