Polymer Property : Charpy Impact, Notched = 1.28 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.270 J/cm²

@Temperature -20.0 °C
1.28 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom PLASTAMID® 610 BT N 32 B PA610
Basic type PA610 for injection molding, modified for general use. Use: extrusion, filaments, injection molding. Delivered in the natural color.Information Provided by Plastcom spol. s r.o.
Charpy Impact, Notched 0.270 J/cm²

@Temperature 23.0 °C
1.28 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVALEN PH 72 T 40 PP, 40% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, thermo stable, chemically modified talc. General application in all industry branches - covers of..
Charpy Impact, Notched 0.270 J/cm²

@Temperature 23.0 °C
1.28 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6 GF 10 GB 20 PA6, 10% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and..
Charpy Impact, Notched 0.270 J/cm²

@Temperature 23.0 °C
1.28 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6 GF 10 TS PA6, 10% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and..
Charpy Impact, Notched 0.270 J/cm²

@Temperature -30.0 °C
1.28 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® S CP300 (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact, Notched 0.270 J/cm²

@Temperature -20.0 °C
1.28 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 1-8000 Polypropylene Homopolymer
INNOPOL® CS 1-8000 is a polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-8000 is highly suitable for manufacturing indoor waste wate..