Inno-Comp INNOPOL® CS 1-8000 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Inno-Comp Ltd
Trade Name INNOPOL® CS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Inno-Comp INNOPOL® CS 1-8000 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INNOPOL® CS 1-8000 is a polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-8000 is highly suitable for manufacturing indoor waste water discharge system and chemical treated parts, where the required properties are high strength, high stiffness and chemical resistance.All information provided by INNO-COMP.
Physical Properties Metric English Comments
Density 0.900 g/cc

@Temperature 23.0 °C
0.0325 lb/in³

@Temperature 73.4 °F
ISO 1183
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
50 mm/min; ISO 527-1,-2
Elongation at Yield 11 %
11 %
50 mm/min; ISO 527-1,-2
Tensile Modulus 1.30 GPa
189 ksi
1 mm/min; ISO 527-1,-2
Izod Impact, Notched (ISO) 3.10 kJ/m²

@Temperature -20.0 °C
1.48 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
12.0 kJ/m²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Charpy Impact, Notched 0.270 J/cm²

@Temperature -20.0 °C
1.28 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 164 °C
327 °F
DSC; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
ISO 75-1,-2
Descriptive Properties Value Comments
Color Natural