Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 4401R PPC+PC LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 4404 PPC+PC High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® BFL2000 PC (Asia Pacific) Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® BPL1000 PC Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Asia Pacific) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature -40.0 °C |
11.2 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL8483 PC COPOLYMER (Asia Pacific) Lexan* EXL8483 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 80% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX2414G PC (Asia Pacific) 10 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
LATI LASTANE 50 G/40 40% Glass Fiber Reinforced Polyurethane (PUR)
(discontinued **) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Izod Impact, Notched | 6.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
11.2 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH830 Flame Retardant PC Features:UL V-0 @ 1.6mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInformation Prov.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
Ineos G36-10-150 HDPE G36-10-150 is a medium density hexene copolymer polyethylene resin designed for the blown geomembrane sheet process. This resin is especially well suited for the production of textured geomembranes... |
|||
Izod Impact, Notched | >= 6.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 11.2 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa LONOY 2200 HT PC/PET Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
Ineos K44-06-122 HDPE HDPE K44-06-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as .. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 0.000 °C |
11.2 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature -30.0 °C |
11.2 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature -30.0 °C |
11.2 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Asia Pacific) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature -30.0 °C |
11.2 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Europe-Africa-Middle East) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature -30.0 °C |
11.2 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Asia Pacific) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature -30.0 °C |
11.2 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East) XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SPS Guang Zhou POLOYâ„¢ 2002(+) Flame-retarded PC/ABS Characteristic: Good flame retardance, good mechanical properties and good machining propertiesApplications: Communication products, audio and video productsInformation Provided by SPS (Guang Zhou) .. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
Styrolution Luran® S 796 M Colored ASA Description: High-impact injection molding gr4ade with good flowability.Applications: Trim panels for goods vehicles.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
Styrolution Luran® S 797 S UV White 33999 Q455 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
Styrolution Luran® S 797 S White 35962 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP NX10302 PC+ABS (Asia Pacific) This is a PC/ABS compound with improved plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamOfin PPC717 Polypropylene, UV Stabilized UV stabilized polypropylene copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2173HU Toyota High Impact Copolymer Polypropylene DescriptionPolyfort® PP 2173HU Toyota is a high flow, UV stabilized, high impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
E-Polymers Tekaloy® G70A2 Impact Resistance, Easy Molding PC/ABS Alloy Impact Resistance, Easy MoldingInformation provided by E-Polymers Co. Ltd. |