Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.214 - 2.98984 J/cm @Temperature -20.0 - 4.00 °C |
0.401 - 5.60120 ft-lb/in @Temperature -4.00 - 39.2 °F |
Average value: 1.14 J/cm Grade Count:7 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |