Polymer Property : Izod Impact, Notched = 4.53 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.53 J/cm
8.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycolac® MG29 ABS
Super high impact ABS. Good low temperature toughness. High gloss.
Izod Impact, Notched 4.53 J/cm
8.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycolac® MG29 ABS (Asia Pacific)
Super high impact ABS. Good low temperature toughness. High gloss.
Izod Impact, Notched 4.53 J/cm
8.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycoloy® C2950HF PC+ABS
Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced impact and heat properties plus improved flow for various applications.
Izod Impact, Notched 4.53 J/cm
8.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL STN15HF PPE+PS
Automotive interiors. Improved flow characteristics/overall processing economy. 240F DTUL. High impact/good property retention after heat ageing.
Izod Impact, Notched 4.53 J/cm
8.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL STN15HF PPE+PS (Asia Pacific)
Automotive interiors. Improved flow characteristics/overall processing economy. 240F DTUL. High impact/good property retention after heat ageing.
Izod Impact, Notched 4.53 J/cm

@Thickness 3.20 mm
8.49 ft-lb/in

@Thickness 0.126 in
ASTM D256
SABIC Innovative Plastics ULTEM 2210 PEI
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
Izod Impact, Notched 4.53 J/cm

@Thickness 3.20 mm
8.49 ft-lb/in

@Thickness 0.126 in
ASTM D256
SABIC Innovative Plastics ULTEM 2210 PEI (Asia Pacific)
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
Izod Impact, Notched 4.53 J/cm
8.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRILOY D2000P PC
LNP LUBRILOY* D2000P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Exceptional Processing, Wear Resistant.
Izod Impact, Notched 4.53 J/cm
8.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRILOY D2000P PC (Asia Pacific)
LNP LUBRILOY* D2000P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Exceptional Processing.
Izod Impact, Notched 4.53 J/cm
8.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL EM6100 PPE+PS
PPE+PS blend. Unfilled. Good balance of flow/heat/impact. Dimensional stability. Paint adhesion. Suitable for the automotive interior market: HVAC housings, radio components. MS-DB424, WSB-M4D844-A9..
Izod Impact, Notched 4.53 J/cm
8.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL EM6100 PPE+PS (Asia Pacific)
Medium heat, high impact PPO/HIPS alloy used in the automotive industry.