Polymer Property : Izod Impact, Notched = 4.41 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.41 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
8.27 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY GP5006AF PC/ABS, Flame Retardant
Description: Injection Molding, PC/ABS, Flame RetardantApplication: Electric and Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chem..
Izod Impact, Notched 4.41 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
8.27 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUTENE-H BE0350 HDPE
Description: LUTENE-H BE0350 is an excellent material for blow-molded articles with high density and rigidity. It has good flow characteristics, high parison stability and impact resistance.Applicat..
Izod Impact, Notched >= 4.41 J/cm

@Thickness 6.35 mm
>= 8.27 ft-lb/in

@Thickness 0.250 in
ASTM D256
Gromax CCP PBT 1100-220S
Product Description: PBT unreinforced and impact-modified injection molding grade. Characteristics:Low warp age, high toughness and excellent dimensional stabilityExcellent glossy surface and less-g..
Izod Impact, Notched 4.41 J/cm

@Thickness 3.17 mm
8.27 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® HI-1001B PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 4.41 J/cm

@Thickness 6.35 mm
8.27 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Infino® HP-1000XA PC/ABS, Unreinforced
PC/ABS material for automobile IP-coreInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 4.41 J/cm

@Thickness 3.17 mm
8.27 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® HI-1001B PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 4.41 J/cm

@Thickness 6.35 mm
8.27 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Infino® HP-1000XA PC/ABS, Unreinforced
PC/ABS material for automobile IP-coreInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 4.41 J/cm
8.27 ft-lb/in
ASTM D256
E-Polymers TEKALOY® G70NHT Non Halogen Flame Retardant Impact Resistance PC/ABS Alloy
PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistan..
Izod Impact, Notched 4.41 J/cm

@Thickness 3.20 mm
8.27 ft-lb/in

@Thickness 0.126 in
ASTM D-256
Bhansali Engineering Abstron IMC-45 FR V2 Flame Retardant PC/ABS Grade
Information provided by Bhansali
Izod Impact, Notched 4.41 J/cm

@Thickness 3.20 mm
8.27 ft-lb/in

@Thickness 0.126 in
ASTM D-256
Bhansali Engineering Abstron IMC-45 FR V2 Flame Retardant PC/ABS Grade
Information provided by Bhansali