Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.36 J/cm @Thickness 3.17 mm |
6.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF30 IM HS L 30% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI.. |
|||
Izod Impact, Notched | 3.36 J/cm | 6.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP YF005 TPEE (Asia Pacific) LNP* Thermocomp* YF005 is a compound based on TPEE resin containing Glass Fiber. |
|||
Izod Impact, Notched | 3.36 J/cm | 6.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX626 PPE+PS+PA Blowmolding and extrusion. High heat and chemical resistant. |