Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP YF005 TPEE (Asia Pacific)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP YF005 TPEE (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* YF005 is a compound based on TPEE resin containing Glass Fiber.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Time 86400 sec
0.0040 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 54.0 MPa
7830 psi
ASTM D638
Elongation at Break 8.5 %
8.5 %
ASTM D638
Tensile Modulus 2.73 GPa
396 ksi
50 mm/min; ASTM D638
Flexural Strength 68.0 MPa
9860 psi
ASTM D790
Flexural Modulus 2.53 GPa
367 ksi
ASTM D790
Izod Impact, Notched 3.36 J/cm
6.29 ft-lb/in
ASTM D256
Izod Impact, Unnotched 12.5 J/cm
23.4 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 170 °C

@Thickness 3.20 mm
338 °F

@Thickness 0.126 in
unannealed; ASTM D648