Mechanical Properties Metric English Comments
Izod Impact, Notched 1.38 J/cm
2.59 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP DFL38 PC
LNP* Lubricomp* DFL-4038 is a Polycarbonate containing 40% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated.
Izod Impact, Notched 1.38 J/cm
2.59 ft-lb/in
ASTM D256
Flint Hills 23T2A Random Copolymer Polypropylene
Features: Clarified, autoclave and good impact strength. Product does not contain animal derived components.Applications: Designed for Blow molding and ThermoformingInformation provided by Flint H..
Izod Impact, Notched 1.38 J/cm
2.59 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP IFL36 PA6.12
LNP LUBRICOMP* IFL36 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
Izod Impact, Notched 1.38 J/cm
2.59 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66
LNP* LUBRICOMP* RFP36 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE, Silicone. Added features of this material include: Wear Resistant.
Izod Impact, Notched 1.38 J/cm
2.59 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 (Asia Pacific)
LNP* Lubricomp* RFP36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. This product is also known as Lub..
Izod Impact, Notched 1.38 J/cm
2.59 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP RFP36S PA 66
LNP* LUBRICOMP* RFP36S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Heat Stabilized.
Izod Impact, Notched 1.38 J/cm
2.59 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP RFP36XXZ PA 66 (Asia Pacific)
LNP Lubricomp RFP36XXZ is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: internally lubricated. Also known as Lubricomp RFL-4536 ..
Izod Impact, Notched 1.38 J/cm

@Temperature 23.0 °C
2.59 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp DF0069E PC
LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC..
Izod Impact, Notched 1.38 J/cm

@Temperature 23.0 °C
2.59 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp DF0069E PC (Asia Pacific)
LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC..
Izod Impact, Notched 1.38 J/cm
2.59 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA 6/12
LNP THERMOCOMP* IF006 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber.
Izod Impact, Notched 1.38 J/cm

@Temperature 23.0 °C
2.59 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp IF006S PA 6/12 (Asia Pacific)
LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci..
Izod Impact, Notched 1.38 J/cm
2.59 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10 (Asia Pacific)
LNP* Thermocomp* QF007 is a compound based on Nylon 6/10 resin containing Glass Fiber.
Izod Impact, Notched 1.38 J/cm
2.59 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP QF008 PA 6/10 (Asia Pacific)
LNP* Thermocomp* QF008 is a compound based on Nylon 6/10 resin containing Glass Fiber.
Izod Impact, Notched 1.38 J/cm
2.59 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP QF008 PA6.10
LNP* THERMOCOMP* QF008 is a compound based on Nylon 6/10 resin containing 40% Glass Fiber.
Izod Impact, Notched 1.38 J/cm

@Temperature 23.0 °C
2.59 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp QF008R PA 6/10
LNP* Thermocomp* QF008R is a compound based on Nylon 6/10 containing Glass Fiber. Characteristics of this grade are: Easy Release.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 1.38 J/cm
2.59 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP PX92248 PA 6
LNP* THERMOCOMP* PX92248 is a compound based on Nylon 6 resin containing Proprietary Filler(s).
Izod Impact, Notched 1.38 J/cm
2.59 ft-lb/in
ISO 180
Azoty Tarnow™ TARFLEN SG-1 PTFE
Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Izod Impact, Notched 1.38 J/cm
2.59 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC (Asia Pacific)
LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated.
Izod Impact, Notched 1.38 J/cm

@Temperature 23.0 °C
2.59 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp IF006S PA6.12
LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas ..
Izod Impact, Notched 1.38 J/cm
2.59 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC
LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Internally Lubricated.