SABIC Innovative Plastics LNP LUBRICOMP DFL38 PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DFL38 PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* DFL-4038 is a Polycarbonate containing 40% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated.
Physical Properties Metric English Comments
Specific Gravity 1.70 g/cc
1.70 g/cc
ASTM D792
Density 1.69 g/cc
0.0611 lb/in³
ASTM D792
Moisture Absorption 0.0600 %
0.0600 %
50% RH, 24 hrs; ASTM D570
0.0900 %
0.0900 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm

@Time 86400 sec
0.0010 - 0.0030 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm

@Time 86400 sec
0.0030 - 0.0050 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 102 MPa
14800 psi
Type I, 5 mm/min; ASTM D638
127 MPa
18400 psi
5 mm/min; ISO 527
Tensile Strength, Yield 102 MPa
14800 psi
Type I, 5 mm/min; ASTM D638
127 MPa
18400 psi
5 mm/min; ISO 527
Elongation at Break 1.8 %
1.8 %
Type I, 5 mm/min; ASTM D638
1.9 %
1.9 %
5 mm/min; ISO 527
Elongation at Yield 1.8 %
1.8 %
Type I, 5 mm/min; ASTM D638
1.9 %
1.9 %
5 mm/min; ISO 527
Tensile Modulus 11.76 GPa
1706 ksi
5 mm/min; ASTM D638
12.88 GPa
1868 ksi
1 mm/min; ISO 527
Flexural Strength 192 MPa
27800 psi
ISO 178
196 MPa
28400 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Yield Strength 196 MPa
28400 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 11.56 GPa
1677 ksi
2 mm/min; ISO 178
12.1 GPa
1750 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.38 J/cm
2.59 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.47 J/cm
12.1 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 42.0 kJ/m²
20.0 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
Coefficient of Friction, Dynamic 0.48
0.48
ASTM D3702 Modified
Coefficient of Friction, Static 0.51
0.51
ASTM D3702 Modified
K (wear) Factor 46.3 x 10-8 mm³/N-M
23.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 29.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
21.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
143 °C

@Thickness 3.20 mm
289 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
137 °C

@Thickness 3.20 mm
279 °F

@Thickness 0.126 in
unannealed; ASTM D648