Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.36 J/cm | 2.54 ft-lb/in | ASTM D 256 |
Shakespeare Isocorâ„¢ HZ73SI high viscosity PA-6 Isocorâ„¢ HZ73SI is a high viscosity PA-6. This resin is specifically suited for applications requiring excellent abrasion, tensile and elongation properties. This resin can be processed using.. |
|||
Izod Impact, Notched | 1.36 J/cm | 2.54 ft-lb/in | ASTM D 256 |
Shakespeare Isocorâ„¢ SVP4007 Nylon 6 Isocorâ„¢ SVP4007 is a high viscosity PA-6. This resin is specifically suited for applications requiring excellent abrasion, tensile and elongation properties. This resin can be processed usin.. |