Shakespeare Isocorâ„¢ SVP4007 Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Shakespeare Company
Trade Name Isocor™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare Isocorâ„¢ SVP4007 Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Isocorâ„¢ SVP4007 is a high viscosity PA-6. This resin is specifically suited for applications requiring excellent abrasion, tensile and elongation properties. This resin can be processed using conventional techniques. Used for profile extrusions, film extrusions, flexible tubing, fiber and filaments.Information provided by Shakespeare Company.
Physical Properties Metric English Comments
Density 1.103 g/cc
0.03985 lb/in³
ASTM D 792
Linear Mold Shrinkage 0.015 cm/cm

@Thickness 3.17 mm
0.015 in/in

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Tensile Strength at Break 52.6 MPa
7630 psi
ASTM D 638
Tensile Modulus 1.87 GPa
271 ksi
ASTM D 638
Izod Impact, Notched 1.36 J/cm
2.54 ft-lb/in
ASTM D 256
Gardner Impact 36.2 J

@Temperature 23.0 °C
26.7 ft-lb

@Temperature 73.4 °F
ASTM 5420
Thermal Properties Metric English Comments
Melting Point 213 °C
415 °F
DSC
Glass Transition Temp, Tg 120 °C
248 °F
DSC