Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.36 J/cm @Temperature -30.0 °C |
2.55 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HP9NR PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. For blow molding .. |
|||
Izod Impact, Notched | 1.36 J/cm @Temperature 0.000 °C |
2.55 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics GELOY XTPM405 ASA+PC High flow PC/ASA with improved impact at room and low temperatures. Improved release. Excellent weatherability for outdoor unpainted or clearcoated applications. Injection Moldable with large color .. |
|||
Izod Impact, Notched | 1.36 J/cm | 2.54 ft-lb/in | ASTM D 256 |
Shakespeare Isocorâ„¢ HZ73SI high viscosity PA-6 Isocorâ„¢ HZ73SI is a high viscosity PA-6. This resin is specifically suited for applications requiring excellent abrasion, tensile and elongation properties. This resin can be processed using.. |
|||
Izod Impact, Notched | 1.36 J/cm | 2.54 ft-lb/in | ASTM D 256 |
Shakespeare Isocorâ„¢ SVP4007 Nylon 6 Isocorâ„¢ SVP4007 is a high viscosity PA-6. This resin is specifically suited for applications requiring excellent abrasion, tensile and elongation properties. This resin can be processed usin.. |
|||
Izod Impact, Notched | 1.36 J/cm | 2.55 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DD0009XP PC LNP* STAT-KON* D-FR is a compound based on Polycarbonate resin containing Carbon. Added features of this grade include: Flame Retardant, Electrically Conductive. |