Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kleerdex Kydex® 120 Acrylic/PVC Thermoplastic Sheet  (discontinued **)

Category Polymer , Thermoplastic , Acrylic (PMMA) , Vinyl (PVC) , PVC/Acrylic Alloy
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kleerdex Kydex® 120 Acrylic/PVC Thermoplastic Sheet  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
USDA approved thermoplastic sheetApplications: High impact resistant wallcovering, push plates and kick plates, equipment housings, splash and safety guardsFeatures: Kydex 120 meets class I/A fire codes when used as a protective wallcoverings and meets UL Standard 94 V-0/5V fire ratings in all thickness, the highest listing for flame retardant plastic components. It is tough, impact and scratch resistant, Kydex 120 will provide years of service when formed into plastic components or used as a wallcovering. In food processing environments where cleanliness is essential, Kydex 120 is more resistant to a wider range of cleaners than other thermoplastics. It also resists staining from foodstuffs.Fabrication: Excellent forming properties result in uniform wall thicknesses and crisp detail, plus easy machining and fabricating using conventional methods, further expanding finished part possibilities.Data provided by the Kleerdex Company.Kleerdex Company became KYDEX, LLC in 2009.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ASTM D785
Tensile Strength, Ultimate 42.0 MPa
6090 psi
ASTM D638
Elongation at Break 160 %
160 %
Modulus of Elasticity 2.31 GPa
335 ksi
Flexural Yield Strength 64.0 MPa
9280 psi
ASTM D790
Izod Impact, Notched 9.53 J/cm

@Temperature 23.0 °C
17.9 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Taber Abrasion, mg/1000 Cycles 0.038
0.038
ASTM D1044
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
annealed; ASTM D648
Flammability, UL94 V-0
V-0
V-0, 5V; UL Standard 94
Processing Properties Metric English Comments
Processing Temperature 162 - 200 °C
324 - 392 °F
Forming Temperature