Polymer Property : Izod Impact, Notched = 15.6 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 7.26 - 8.33 J/cm
13.6 - 15.6 ft-lb/in
Bulk Molding Compounds BMC T44 High Strength Mineral Filled Molding Compound
BMC T44 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displacing ..
Izod Impact, Notched 7.26 - 8.33 J/cm
13.6 - 15.6 ft-lb/in
Bulk Molding Compounds BMC T44-15613 High Strength Mineral Filled Molding Compound
BMC T44-15613 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displ..
Izod Impact, Notched 0.502 - 8.33 J/cm
0.940 - 15.6 ft-lb/in
Average value: 3.63 J/cm Grade Count:7
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..