Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.26 - 8.33 J/cm | 13.6 - 15.6 ft-lb/in | |
Bulk Molding Compounds BMC T44 High Strength Mineral Filled Molding Compound BMC T44 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displacing .. |
|||
Izod Impact, Notched | 7.26 - 8.33 J/cm | 13.6 - 15.6 ft-lb/in | |
Bulk Molding Compounds BMC T44-15613 High Strength Mineral Filled Molding Compound BMC T44-15613 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displ.. |