Polymer Property : Izod Impact, Notched = 13.2 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 7.05 J/cm
13.2 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Network Polymers NPP 25-0414
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Izod Impact, Notched 7.05 J/cm
13.2 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Network Polymers NPP 25-0616
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Izod Impact, Notched 7.05 J/cm
13.2 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Network Polymers NPP 25-061601
Description: Impact Modified PolypropyleneInformation provided by Network Polymers Inc.
Izod Impact, Notched 7.02 J/cm
13.2 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer
Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char..
Izod Impact, Notched 7.02 J/cm
13.2 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Asia Pacific)
Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char..
Izod Impact, Notched 7.02 J/cm
13.2 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char..
Izod Impact, Notched 7.02 J/cm
13.2 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer
Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin..
Izod Impact, Notched 7.02 J/cm
13.2 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Asia Pacific)
Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin..
Izod Impact, Notched 7.02 J/cm
13.2 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin..
Izod Impact, Notched 7.02 J/cm
13.2 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
Izod Impact, Notched 7.02 J/cm
13.2 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific)
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
Izod Impact, Notched 7.02 J/cm
13.2 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® HPX8REU PC Copolymer (Europe-Africa-Middle East)
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
Izod Impact, Notched 7.02 J/cm
13.2 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® HPXS8R PC Copolymer
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
Izod Impact, Notched 7.06 J/cm

@Thickness 3.17 mm
13.2 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® AE-2030 PC/PET, General Purpose
PC/PET material used for automobile radiator grills and door handlesInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 7.06 J/cm

@Thickness 3.17 mm
13.2 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® AE-2030 PC/PET, General Purpose
PC/PET material used for automobile radiator grills and door handlesInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 7.05 J/cm

@Thickness 3.17 mm
13.2 ft-lb/in

@Thickness 0.125 in
ASTM D256
Diamond Polymers NPP25-0616 Black Impact Modified Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.