Network Polymers NPP 25-0414

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers NPP 25-0414.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.5 MPa
3120 psi
2 in per min; ASTM D638
Elongation at Yield 15 %
15 %
chs 2 in/min; ASTM D638
Flexural Modulus 0.965 GPa
140 ksi
Test Method I, Procedure B (chs speed 0.05 in/min), 1% Tangent; ASTM D790
Izod Impact, Notched 7.05 J/cm
13.2 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Gardner Impact 30.4 J

@Temperature -22.0 °C
22.4 ft-lb

@Temperature -7.60 °F
Gardner
Copyright © lookpolymers.com All Rights Reserved