Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.06 J/cm @Thickness 3.17 mm |
13.2 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® AE-2030 PC/PET, General Purpose PC/PET material used for automobile radiator grills and door handlesInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 7.06 J/cm @Thickness 3.17 mm |
13.2 ft-lb/in @Thickness 0.125 in |
ASTM D256 |