Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 12.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
22.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging 2160 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 12.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
22.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging JGR-154A Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 12.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
22.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging UV-SORB-1 Polyvinyl Chloride, Rigid (PVC, Rigid) Caution: To be used as an additive only.Bottles produced from blends of OxyClear UV-SORB-1 are specifically designed for use where UV sensitive products are being packaged. Dependent on the base Oxy.. |
|||
Izod Impact, Notched | 12.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
22.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging VB7 White 215 Polyvinyl Chloride, Rigid (PVC, Rigid) A rigid PVC Compound designed for extrusion blow molding balusters for railings.Information provided by PolyOne |
|||
Izod Impact, Notched | 12.0 J/cm @Temperature 23.0 °C |
22.5 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Oxford Polymers OPX8320 Polybutylene Terephthalate (PBT), Impact Modified/ Glass Beads Polybutylene Terephthalate (PBT), Impact Modified/ Glass BeadsInformation provided by Oxford Polymers. |
|||
Izod Impact, Notched | 12.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
22.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Dry Blend E7130 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 12.0 J/cm @Thickness 6.35 mm |
22.5 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Nitriflex Nitrimpact 1300 MBS Modifier NITRIMPACT™ 1300 thermoplastic resin is a methyl methacrylate-butadiene-styrene (MBS) impact modifier for transparent and opaque PVC applications. Applications: Transparent PVC Compounds (no use re.. |
|||
Izod Impact, Notched | 12.0 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
22.5 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
Notched V 10 mm; ASTM D256 |
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer
(discontinued **) Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i.. |