Oxford Polymers OPX8320 Polybutylene Terephthalate (PBT), Impact Modified/ Glass Beads

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Bead Filled
Manufacturer Oxford Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers OPX8320 Polybutylene Terephthalate (PBT), Impact Modified/ Glass Beads.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polybutylene Terephthalate (PBT), Impact Modified/ Glass BeadsInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.1 MPa
6400 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 12.0 J/cm

@Temperature 23.0 °C
22.5 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.8 °C
145 °F
ASTM D648