Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Packaging UV-SORB-1 Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Packaging UV-SORB-1 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Caution: To be used as an additive only.Bottles produced from blends of OxyClear UV-SORB-1 are specifically designed for use where UV sensitive products are being packaged. Dependent on the base Oxy Compound used, they may be used for either food contact or general purpose applications.Generally, additions of 4% to 10 % by Polymer weight, are recommended in order to comply with FDA Status.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Density 0.801 g/cc
0.0289 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Hardness, Shore D 83
83
ASTM D2240
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.69 GPa
390 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 77.9 MPa
11300 psi
ASTM D790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 12.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
22.5 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C

@Thickness 3.18 mm
149 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Mold Temperature 202 - 213 °C
396 - 415 °F
Blow Molding
Descriptive Properties Value Comments
Additive UV Stabilizer
Agency Ratings FDA Food Contact, Unspecified Rating
Appearance Clear/Transparent
Features Food Contact Acceptable
High Gloss
High Impact Resistance
UV Absorbing
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Blow Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Bottles
Packaging
Copyright © lookpolymers.com All Rights Reserved