Polymer Property : Izod Impact, Notched = 1.95 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.04 J/cm
1.95 ft-lb/in
ASTM D256
Ineos Nova 782 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
High flow, Custom colorsApplications: Multi-purpose injection molding where custom color is a requirement, Toys, Appliance, Computer peripheralsPerformance grades of polystyrene are engineered to ha..
Izod Impact, Notched 1.04 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.95 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Kingfa FRHIPS-960 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance properties, Non-DPOGood heat stabilityColor tailor-made for clientApplications:Injection moldingGas assistant moldingPrinter and photocopier ..
Izod Impact, Notched 1.04 J/cm

@Thickness 3.20 mm
1.95 ft-lb/in

@Thickness 0.126 in
ASTM D256
KKPC Kuhmo HI 425EH Extrusion Molding HIPS
Key features: ESCR Common Uses: Refrigerator inner liners, door liners, disposable cups, food packaging sheet, wrapping films, trays, washing machinesHIPS is a functional resin made by copolymerizat..
Izod Impact, Notched 1.04 J/cm
1.95 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP QC006 PA6.10
LNP THERMOCOMP* QC006 is a compound based on Nylon 6/10 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Notched 1.04 J/cm
1.95 ft-lb/in
0.5 in.; ASTM D256
Resirene Resirene® 6110 High Impact Polystyrene
Features:High ImpactEasy ProcessingFDA Rating: 21 CFR 177.1640FlexibilityApplications:Injection MoldingTV CabinetsRemote ControlsToysInformation provided by US distributor Calsak Corporation.