Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.04 J/cm | 1.95 ft-lb/in | ASTM D256 |
Ineos Nova 782 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Custom colorsApplications: Multi-purpose injection molding where custom color is a requirement, Toys, Appliance, Computer peripheralsPerformance grades of polystyrene are engineered to ha.. |
|||
Izod Impact, Notched | 1.04 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.95 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa FRHIPS-960 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance properties, Non-DPOGood heat stabilityColor tailor-made for clientApplications:Injection moldingGas assistant moldingPrinter and photocopier .. |
|||
Izod Impact, Notched | 1.04 J/cm @Thickness 3.20 mm |
1.95 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
KKPC Kuhmo HI 425EH Extrusion Molding HIPS Key features: ESCR Common Uses: Refrigerator inner liners, door liners, disposable cups, food packaging sheet, wrapping films, trays, washing machinesHIPS is a functional resin made by copolymerizat.. |
|||
Izod Impact, Notched | 1.04 J/cm | 1.95 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP QC006 PA6.10 LNP THERMOCOMP* QC006 is a compound based on Nylon 6/10 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 1.04 J/cm | 1.95 ft-lb/in | 0.5 in.; ASTM D256 |
Resirene Resirene® 6110 High Impact Polystyrene Features:High ImpactEasy ProcessingFDA Rating: 21 CFR 177.1640FlexibilityApplications:Injection MoldingTV CabinetsRemote ControlsToysInformation provided by US distributor Calsak Corporation. |