Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.784532 - 0.980665 J/cm @Temperature -40.0 - -30.0 °C |
1.46975 - 1.83719 ft-lb/in @Temperature -40.0 - -22.0 °F |
Average value: 1.21 J/cm Grade Count:1 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 0.784532 - 0.980665 J/cm @Thickness 3.20 - 3.20 mm |
1.46975 - 1.83719 ft-lb/in @Thickness 0.126 - 0.126 in |
Average value: 1.21 J/cm Grade Count:1 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 0.784532 - 0.882598 J/cm @Temperature -30.0 - -30.0 °C |
1.46975 - 1.65347 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 1.23 J/cm Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||
Izod Impact, Notched | 0.784532 - 0.882598 J/cm @Thickness 3.17 - 6.35 mm |
1.46975 - 1.65347 ft-lb/in @Thickness 0.125 - 0.250 in |
Average value: 1.23 J/cm Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |