Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.784532 - 0.882598 J/cm

@Temperature -30.0 - -30.0 °C
1.46975 - 1.65347 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 1.23 J/cm Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..
Izod Impact, Notched 0.784532 - 0.882598 J/cm

@Thickness 3.17 - 6.35 mm
1.46975 - 1.65347 ft-lb/in

@Thickness 0.125 - 0.250 in
Average value: 1.23 J/cm Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..