Polymer Property : Izod Impact, Notched = 0.784532 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.784532 - 0.980665 J/cm

@Temperature -40.0 - -30.0 °C
1.46975 - 1.83719 ft-lb/in

@Temperature -40.0 - -22.0 °F
Average value: 1.21 J/cm Grade Count:1
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..
Izod Impact, Notched 0.784532 - 0.980665 J/cm

@Thickness 3.20 - 3.20 mm
1.46975 - 1.83719 ft-lb/in

@Thickness 0.126 - 0.126 in
Average value: 1.21 J/cm Grade Count:1
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..
Izod Impact, Notched 0.784532 - 0.882598 J/cm

@Temperature -30.0 - -30.0 °C
1.46975 - 1.65347 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 1.23 J/cm Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..
Izod Impact, Notched 0.784532 - 0.882598 J/cm

@Thickness 3.17 - 6.35 mm
1.46975 - 1.65347 ft-lb/in

@Thickness 0.125 - 0.250 in
Average value: 1.23 J/cm Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..