Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.530 - 0.690 J/cm @Thickness 6.35 mm |
0.993 - 1.29 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ PK-000/15T Polyetheretherketone - 15% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.374 - 0.686 J/cm | 0.700 - 1.29 ft-lb/in | Average value: 0.520 J/cm Grade Count:15 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Izod Impact, Notched | 0.430 - 0.690 J/cm @Thickness 6.35 mm |
0.806 - 1.29 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ NL-000/40T Nylon 6/12 - 40% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.370 - 0.690 J/cm @Temperature -40.0 - -40.0 °C |
0.693 - 1.29 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.561 J/cm Grade Count:15 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |