Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® LCP-30GF/000 Liquid Crystal Polymer - 30% Glass Fiber  (discontinued **)

Category Polymer , Thermoplastic , Liquid Crystal Polymer (LCP)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® LCP-30GF/000 Liquid Crystal Polymer - 30% Glass Fiber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
ASTM D792
Water Absorption 0.020 %
0.020 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0015 - 0.0020 cm/cm

@Thickness 3.17 mm
0.0015 - 0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 159 MPa
23100 psi
ASTM D638
Elongation at Break 1.0 - 3.0 %
1.0 - 3.0 %
ASTM D638
Tensile Modulus 14.5 GPa
2100 ksi
ASTM D638
Flexural Yield Strength 214 MPa
31000 psi
ASTM D790
Flexural Modulus 13.1 GPa
1900 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm

@Thickness 6.35 mm
2.40 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
469 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 316 - 343 °C
601 - 649 °F
Stock
Mold Temperature 135 - 149 °C
275 - 300 °F
Drying Temperature 135 - 149 °C
275 - 300 °F