Polymer Property : Izod Impact, Notched = 0.85424 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.196133 - 0.85424 J/cm

@Temperature -30.0 - -18.0 °C
0.367438 - 1.6003 ft-lb/in

@Temperature -22.0 - -0.400 °F
Average value: 0.562 J/cm Grade Count:9
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched 0.196133 - 0.85424 J/cm

@Thickness 3.17 - 6.50 mm
0.367438 - 1.6003 ft-lb/in

@Thickness 0.125 - 0.256 in
Average value: 0.562 J/cm Grade Count:9
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched 0.26695 - 0.85424 J/cm

@Diameter 6.35 - 6.35 mm
0.50011 - 1.6003 ft-lb/in

@Diameter 0.250 - 0.250 in
Average value: 0.463 J/cm Grade Count:6
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Izod Impact, Notched 0.26695 - 0.85424 J/cm

@Temperature 0.000 - 0.000 °C
0.50011 - 1.6003 ft-lb/in

@Temperature 32.0 - 32.0 °F
Average value: 0.463 J/cm Grade Count:6
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Izod Impact, Notched 0.85424 - 0.85424 J/cm

@Temperature -30.0 - -30.0 °C
1.6003 - 1.6003 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.854 J/cm Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..