Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.26695 - 2.93645 J/cm @Temperature -40.0 - -40.0 °C |
0.50011 - 5.50117 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.60 J/cm Grade Count:2 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Izod Impact, Notched | 0.26695 J/cm - NB @Temperature -40.0 - -40.0 °C |
0.50011 ft-lb/in - NB @Temperature -40.0 - -40.0 °F |
Average value: 1.16 J/cm Grade Count:8 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.26695 - 0.85424 J/cm @Diameter 6.35 - 6.35 mm |
0.50011 - 1.6003 ft-lb/in @Diameter 0.250 - 0.250 in |
Average value: 0.463 J/cm Grade Count:6 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.26695 - 0.85424 J/cm @Temperature 0.000 - 0.000 °C |
0.50011 - 1.6003 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.463 J/cm Grade Count:6 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.26695 - 0.800 J/cm @Temperature 0.000 - 0.000 °C |
0.50011 - 1.50 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.516 J/cm Grade Count:3 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.26695 - 0.800 J/cm @Diameter 6.35 - 6.35 mm |
0.50011 - 1.50 ft-lb/in @Diameter 0.250 - 0.250 in |
Average value: 0.516 J/cm Grade Count:3 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |