Izod Impact, Notched 0.250 - 0.380 J/cm
0.468 - 0.712 ft-lb/in
ASTM D256
RedEye On Demand Clear PolyJet™ FC720 for Rapid Prototyping
Clear PolyJet Resin (FC720) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Clear PolyJet Resin material offer..