Polymer Property : Izod Impact, Notched = 0.699 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.699 J/cm
1.31 ft-lb/in
Pyrotek F-51 Dense Machinable Board
F-51 is a high temperature resin base, supplemented with fiberglass and graphite to provide extra strength and lubricity. F-51 is abrasion resistant and suitable for hot glass handling applications..