Pyrotek F-51 Dense Machinable Board

Category Polymer , Thermoset , Filled/Reinforced Thermoset
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek F-51 Dense Machinable Board.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
F-51 is a high temperature resin base, supplemented with fiberglass and graphite to provide extra strength and lubricity. F-51 is abrasion resistant and suitable for hot glass handling applications up to 700°C.ApplicationsContainer dead plates Guide rails Wear pad Donut rollers for glass AdvantagesAbrasion resistant Excellent heat resistance Non-marking to glass Machinable Excellent wear resistance Good physical strength Good shock resistance Information provided by Pyrotek.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 31.0 MPa
4500 psi
Flexural Strength 59.0 MPa
8560 psi
Compressive Strength 59.0 MPa
8560 psi
Shear Strength 57.0 MPa
8270 psi
Izod Impact, Notched 0.699 J/cm
1.31 ft-lb/in
Thermal Properties Metric English Comments
Thermal Conductivity 0.0900 W/m-K
0.625 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 700 °C
1290 °F
Continuous