Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.320 - 0.587 J/cm | 0.600 - 1.10 ft-lb/in | Average value: 0.521 J/cm Grade Count:16 |
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Izod Impact, Notched | 0.374 - 0.587 J/cm | 0.700 - 1.10 ft-lb/in | Average value: 0.486 J/cm Grade Count:9 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% .. |
|||
Izod Impact, Notched | 0.400 - 0.587 J/cm | 0.749 - 1.10 ft-lb/in | Average value: 0.503 J/cm Grade Count:9 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Izod Impact, Notched | 0.160 - 0.587 J/cm | 0.300 - 1.10 ft-lb/in | Average value: 0.322 J/cm Grade Count:8 |
Overview of materials for Acrylic, UV Stabilized, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of.. |