Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.490332 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.490332 - 980.567 J/cm

@Temperature -40.0 - -40.0 °C
0.918594 - 1837.00 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.16 J/cm Grade Count:27
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched 0.490332 - 980.567 J/cm

@Thickness 6.40 - 6.40 mm
0.918594 - 1837.00 ft-lb/in

@Thickness 0.252 - 0.252 in
Average value: 1.16 J/cm Grade Count:27
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched 0.490332 - 0.490332 J/cm

@Temperature 3.20 - 3.20 °C
0.918594 - 0.918594 ft-lb/in

@Temperature 37.8 - 37.8 °F
Average value: 0.427 J/cm Grade Count:1
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched 0.490332 - 0.490332 J/cm

@Thickness 23.0 - 23.0 mm
0.918594 - 0.918594 ft-lb/in

@Thickness 0.906 - 0.906 in
Average value: 0.427 J/cm Grade Count:1
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched 0.490332 - 3.43233 J/cm

@Temperature -20.0 - 0.000 °C
0.918594 - 6.43016 ft-lb/in

@Temperature -4.00 - 32.0 °F
Average value: 1.91 J/cm Grade Count:9
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..
Izod Impact, Notched 0.490332 - 980.567 J/cm

@Temperature -40.0 - -40.0 °C
0.918594 - 1837.00 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.22 J/cm Grade Count:16
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..
Izod Impact, Notched 0.490332 - 980.567 J/cm

@Thickness 3.17 - 3.17 mm
0.918594 - 1837.00 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 1.22 J/cm Grade Count:16
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..
Copyright © lookpolymers.com All Rights Reserved