Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.918594 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.490332 - 0.490332 J/cm

@Temperature 3.20 - 3.20 °C
0.918594 - 0.918594 ft-lb/in

@Temperature 37.8 - 37.8 °F
Average value: 0.427 J/cm Grade Count:1
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched 0.490332 - 0.490332 J/cm

@Thickness 23.0 - 23.0 mm
0.918594 - 0.918594 ft-lb/in

@Thickness 0.906 - 0.906 in
Average value: 0.427 J/cm Grade Count:1
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched 0.392266 - 0.490332 J/cm

@Temperature -30.0 - -30.0 °C
0.734875 - 0.918594 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.468 J/cm Grade Count:5
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched 0.392266 - 0.490332 J/cm

@Thickness 3.20 - 6.40 mm
0.734875 - 0.918594 ft-lb/in

@Thickness 0.126 - 0.252 in
Average value: 0.468 J/cm Grade Count:5
Overview of materials for Polystyrene, Flame Retardant