Mechanical Properties Metric English Comments
Izod Impact, Notched 0.198 - 8.01 J/cm
0.370 - 15.0 ft-lb/in
Average value: 0.688 J/cm Grade Count:159
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Izod Impact, Notched 0.198 J/cm - NB
0.371 ft-lb/in - NB
Average value: 0.346 J/cm Grade Count:27
Overview of materials for Styrene-Butadiene Copolymer, SBC
This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values ..
Izod Impact, Notched 0.198 J/cm

@Thickness 3.20 mm
0.370 ft-lb/in

@Thickness 0.126 in
ASTM D256
KKPC Kuhmo GP 125EB Extrusion Molding GPPS
Key features: PSP Common Uses: Fruit, egg cell.GPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding processability, and stability of dimension.Da..
Izod Impact, Notched 0.198 J/cm
0.371 ft-lb/in
ASTM D 256
Saint-Gobain Meldin® 2211 Bearing
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Ser..
Izod Impact, Notched 0.198 J/cm
0.371 ft-lb/in
ASTM D256
Plenco 1501 Polyester, Pellet, Injection Molded
PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va..
Izod Impact, Notched 0.198 J/cm
0.370 ft-lb/in
Tra-Con Tra-Cast F353 Optically Opaque Casting System
TRA-CAST F353 is an optically opaque, low viscosity, two-part epoxy system recommended for molding, potting, embedding, encapsulating, sealing and casting applications involving fiber optic, optical..
Izod Impact, Notched 0.198 J/cm

@Thickness 3.17 mm
0.371 ft-lb/in

@Thickness 0.125 in
ASTM D256
Diamond Polymers SBS 2160 Clear Styrene Butadiene Copolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 0.198 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
0.371 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D-256
Chevron Phillips K-Resin® KR03BR SBC  (discontinued **)
K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:BottlesMolded boxes and containersMedical devicesPortion packagesBlister packagingFeatures:Good stiffnessGood formabilityGood toughnessExcelle..
Izod Impact, Notched >= 0.198 J/cm
>= 0.370 ft-lb/in
ASTM D256
Buckeye Polymers BP RPP 2012 T BLK Polypropylene, Talc Filled
Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and ..