Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.198 J/cm - NB | 0.371 ft-lb/in - NB | Average value: 0.346 J/cm Grade Count:27 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.198 J/cm | 0.371 ft-lb/in | ASTM D 256 |
Saint-Gobain Meldin® 2211 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Ser.. |
|||
Izod Impact, Notched | 0.198 J/cm | 0.371 ft-lb/in | ASTM D256 |
Plenco 1501 Polyester, Pellet, Injection Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Izod Impact, Notched | 0.198 J/cm @Thickness 3.17 mm |
0.371 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers SBS 2160 Clear Styrene Butadiene Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.198 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
0.371 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D-256 |
Chevron Phillips K-Resin® KR03BR SBC
(discontinued **) K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:BottlesMolded boxes and containersMedical devicesPortion packagesBlister packagingFeatures:Good stiffnessGood formabilityGood toughnessExcelle.. |