Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS LNP* FARADEX* NS003 is a compound based on PC+ABS resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
Kolon SPESIN® KP213HIBL Impact Resistant PBT Compound resin Impact resistant, BLACKApplications: Wiper bladesInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DX00714H PC LNP LUBRICOMP* DX00714H is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Wear Resistant, Healthcare. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DZL34E PC LNP* Lubricomp* DZL34E is a compound based on Polycarbonate resin containing 20% Milled Glass, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 9076 PEI Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY R2000A PA 66 LNP LUBRILOY* R2000A is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM CRS5211R PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 4012G PBT VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature 23.0 °C |
1.39 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supp.. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 735 PBT (Asia Pacific) 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP AF003 ABS (Asia Pacific) LNP* Thermocomp* AF003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF0046P PC LNP* Thermocomp* DF0046P is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features include: Exceptional Processing, Non-Brominated & Non-Chlorinated Flame Retardant. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF0046P PC (Asia Pacific) LNP* Thermocomp* DF0046P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Exceptional Processing, Flame Retardant, Non-Br.. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature 23.0 °C |
1.39 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp DX99721 PC (Asia Pacific) LNP* Thermocomp* DX99721 is a compound based on Polycarbonate resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MX99432 PP LNP* THERMOCOMP* MX99432 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXH PA 66 LNP THERMOCOMP* RF004XXH is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP UC006H PPA LNP THERMOCOMP* UC006H is a compound based on Polyphthalamide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DE003ER PC (Asia Pacific) LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DEI13F PC LNP* STAT-KON* DEI13F is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 2% Silicone. Added features of this material include: Electrically Conductive, Superior Molding, Wear R.. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature 23.0 °C |
1.39 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC (Asia Pacific) LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was supp.. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM AUT230 PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX91077 PC LNP* STAT-KON* DX91077 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Impact Modified. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP UX93847 PPA LNP* Thermocomp* UX93847 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | |
UBE UBEPOL BR15HL HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %) Description: UBEPOL-BR15HL is a linear type of polymer with the high solution viscosity. In case of enlarging the dispersed rubber particle size in |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature 23.0 °C |
1.39 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and is suitable for Rapid Manufacturing. For use with all Sinterstation® Pro and Sinterstation HiQ™ ser.. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |